SSH EN 12350-7:2019/AC:2022

Testimi i betonit të freskët - Pjesa 7: Përmbajtja e ajrit - Metodat me presion

Testing fresh concrete - Part 7: Air content - Pressure methods
31 tet 2023

General information

60.60     31 tet 2023

95.99   

DPS

DPS/KT 104

European Norm

91.100.30  

anglisht  

Buying

Publikuar

Language in which you want to receive the document.

Scope

This document describes two methods for determination of air content of compacted fresh concrete, made with normal weight or relatively dense aggregate and having a declared value of D of the coarsest fraction of aggregates actually used in the concrete (Dmax) not greater than 63 mm.
The test is not suitable for concretes with slumps less than 10 mm according to EN 12350-2.
Neither method is applicable to concretes made with lightweight aggregates, air cooled blast-furnace slag, or aggregates with high porosity, because of the magnitude of the aggregate correction factor, compared with the entrained air content of the concrete.

Life cycle

PREVIOUSLY

PUBLISHED
SSH EN 12350-7:2019

NOW

PUBLISHED
SSH EN 12350-7:2019/AC:2022
60.60 Standard published
31 tet 2023

Related project

Adopted from EN 12350-7:2019/AC:2022 IDENTICAL