This standard specifies the requirements relating to:
Steel FE-PM1802 (X5CrNiCu15-5)
Consumable electrode remelted
Solution treated and precipitation treated
Plate
6 mm ≤ a ≤ 20 mm
1 070 MPa ≤ Rm≤ 1 220 MPa
for aerospace applications.