Applies to magnetically hard materials only. The described method makes use of a closed loop simulating a ring. Two alternative methods are given for intrinsic coercivity up to and including 600 kA/m and one for materials with higher intrinsic coercivity (e.g. rare earth cobalt alloys).
WITHDRAWN
SSH EN 60404-5:2007
95.99
Withdrawal of Standard
12 sht 2023
PUBLISHED
SSH EN 60404-5:2015