Shfuqizuar
The method is based on heating a test portion of a specified volume to a specified temperature, normally 180 °C, in a depression in an electrically heated steel block and determination of the time at which threads can no longer be pulled from the molten product.
WITHDRAWN
ISO 8130-6:1992
95.99
Withdrawal of Standard
23 qer 2021
WITHDRAWN
ISO 8130-6:1992/Amd 1:1998
Pluhur veshes - Pjesa 6: Percaktimi i kohes se mpiksjes se pluhurave veshes xhelformues me nje temperature te dhene
60.60 Standard published