IEC TS 62607-4-9:2026 ED1

Nanomanufacturing - Key control characteristics - Part 4-9: Nano-enabled energy storage - Electrochemical characteristics of carbon nanomaterial for the electrodes of electric double-layer capacitors: Coin cell preparation

Jul 14, 2026

General information

60.60     Jul 14, 2026

IEC

TC 113

Technical Specification

07.120  

English  

Buying

Published

Language in which you want to receive the document.

Scope

IEC TS 62607-4-9:2026, which is a Technical Specification, establishes a standardized method for assembling
• coin-cell EDLCs
in order to characterize the electrochemical key control characteristic of carbon nanomaterials.
The coin-cell EDLC is fabricated through sequential steps: electrode slurry preparation (mixing), coating, rolling, cutting, weighing, and final assembly.
• The document specifies the assembly process and data recording.
• The document is applicable for carbon nanomaterials used in EDLC as active material or conductive agents, such as nanoporous activated carbon, carbon aerogel, carbon nanotube, carbon black, graphene, nano graphite sheet, vapour-grown carbon fibre and so on.
• Typical application areas of this method are research, manufacturer and downstream user to guide material processing and quality control

Life cycle

NOW

PUBLISHED
IEC TS 62607-4-9:2026 ED1
60.60 Standard published
Jul 14, 2026