DPS
Drejtoria e Përgjithshme e Standardizimit
Phone: +355 4 222 62 55
E-mail: info@dps.gov.al
Address: Address: "Reshit Collaku" Str., (nearby ILDKPKI, VI floor), Po.Box 98, Tiranë - Albania

prSSH EN 12390-18:2021+A1:2024

Testing hardened concrete - Part 18: Determination of the chloride migration coefficient

General information

40.20     Feb 10, 2025

40.60    May 7, 2025

DPS

DPS/KT 104

European Norm

91.100.30  

Scope

This document specifies the procedure for obtaining the non-steady-state chloride migration coefficient of specimens of hardened concrete at a specified age (see Annex A). The test procedure does not take into account any interaction of concrete with the saline solution over time. The test result is a durability indicator with respect to the resistance of the concrete investigated against chloride penetration.
The test procedure does not apply to concrete specimens with surface treatments such as silanes.
If the aggregate or any other embedded elements (such as metallic fibres or conducting particles) are electrically conductive, this will influence the magnitude of chloride migration. This fact is taken into account when establishing threshold values. It prevents comparison of chloride migration values between concretes if the aggregates induce a difference of half an order of magnitude (higher or lower) of chloride migration.

Life cycle

NOW

IN_DEVELOPMENT
prSSH EN 12390-18:2021+A1:2024
40.20 DIS ballot initiated: 12 weeks
Feb 10, 2025

Related project

Adopted from EN 12390-18:2021+A1:2024 IDENTICAL

Preview

Only informative sections of projects are publicly available. To view the full content, you will need to members of the committee. If you are a member, please log in to your account by clicking on the "Log in" button.

Login