SSH EN 12350-7:2019

Testing fresh concrete - Part 7: Air content - Pressure methods

Nov 6, 2019

General information

60.60     Jul 15, 2019

DPS

DPS/KT 104

European Norm

91.100.30  

English  

Buying

Published

Language in which you want to receive the document.

Scope

This European Standard describes two methods for determination of air content of compacted fresh concrete, made with normal weight or relatively dense aggregate and having a declared value of D of the coarsest fraction of aggregates actually used in the concrete (Dmax) not greater than 63 mm.

The test is not suitable for concretes with slumps less than 10 mm.

NOTE Neither method is applicable to concretes made with lightweight aggregates, air cooled blast-furnace slag, or aggregates with high porosity, because of the magnitude of the aggregate correction factor, compared with the entrained air content of the concrete.

Life cycle

PREVIOUSLY

Replaces
SSH EN 12350-7:2009

NOW

PUBLISHED
SSH EN 12350-7:2019
60.60 Standard published
Jul 15, 2019

Related project

Adopted from EN 12350-7:2019

Preview

Only informative sections of projects are publicly available. To view the full content, you will need to members of the committee. If you are a member, please log in to your account by clicking on the "Log in" button.

Login